Research Article

CO2 Induced Foaming Behavior of Polystyrene near the Glass Transition

Figure 2

Photographs of samples of PS depressurized after holding for different times (30 to 180 min) at 100°C and 54 bar (1 mm thickness × 20 mm diameter).