Research Article

CO2 Induced Foaming Behavior of Polystyrene near the Glass Transition

Figure 9

Photographs of a 1 mm thick PS sample at various times after the onset of depressurization after holding at 83 bar (in CO2) and 70°C for 2 hours (scale of images is 6 × 6 mm).