Turning Wood Autohydrolysate Directly into Food Packing Composite Films with Good Toughness
Table 1
The composite films prepared by different volume ratios of WH, CS, and CNC.
| Sample name | Proportion |
| F0.01 | (WH)/(CS)/(CNC) = 1 : 1 : 0.01 | F0.03 | (WH)/(CS)/(CNC) = 1 : 1 : 0.03 | F0.05 | (WH)/(CS)/(CNC) = 1 : 1 : 0.05 | F0.08 | (WH)/(CS)/(CNC) = 1 : 1 : 0.08 | F0.1 | (WH)/(CS)/(CNC) = 1 : 1 : 0.1 |
|
|