Thermal data obtained from TGA thermograms of TPNR and TPNR/RWS composites.

FormulationTemperature at different weight loss (°C)Temperature for maximum weight loss
1st peak2nd peak3rd peak4th peak

Pure NR361.8374.9385.6402.7378.1
Pure HDPE456.9473.5485.2493.9491.0
R6P4373.9393.8450.4466.1379.2467.1
R5P5381.1401.4466.0485.6387.8487.3
R4P6389.5460.8476.5486.7382.7485.1
R3P7392.4464.5479.7489.1382.1486.3
R6P4W30L357.7383.1426.8487.9159.2311.3382.3491.3
R6P4W60L335.1370.6408.2494.8156.5305.2368.8491.9
R4P6W30L365.5394.4475.2494.5162.1300.8383.7493.5
R4P6W60L334.1371.0456.3498.6162.8298.4367.9492.6
R4P6W30S362.8393.1476.4495.0164.4302.3376.4493.9