Research Article
Fatigue Fracture Properties and Morphology of Polyoxymethylene (POM) Plates Produced under Moderate Processing Conditions
Table 8
DSC crystallinity of compression- and injection-molded POM plates.
| Sample position | Crystallinity (%) | Standard deviation (%) |
| Delrin_CM_M | 73.3 | 2.9 | Delrin_IM_90°C-MT_S1 | 70.5 | 2.2 | Delrin_IM_90°C-MT_S2 | 71.2 | 2.8 | Delrin_IM_90°C-MT_S3 | 69.0 | 2.8 |
| Tenac_CM_M | 71.5 | 2.6 | Tenac_IM_90°C-MT_S1 | 67.3 | 1.9 | Tenac_IM_90°C-MT_S2 | 67.7 | 1.8 | Tenac_IM_90°C-MT_S3 | 67.1 | 1.7 |
|
|