Research Article
Hybrid and Nonhybrid Laminate Composites of Sugar Palm and Glass Fibre-Reinforced Polypropylene: Effect of Alkali and Sodium Bicarbonate Treatments
Table 4
Tensile properties of the hybrid and nonhybrid composites.
| Tensile properties | Neat PP | GF/PP | Nonhybrid SPF/PP | Hybrid (sandwich) GF2/SPF2/GF2 | L00 | L01 | L02 | L03 | L04 | L05 | L06 | L07 |