Effects of Size of Zinc Borate on the Flame Retardant Properties of Intumescent Coatings

Table 4

TGA data of IFR/ZB coatings (under nitrogen).

(°C) (°C) (°C) (°C) (°C)W600°C (%)W700°C (%)W800°C (%)

Control IFR13825336242460930.1915.387.23
ZBS2%12425638542762030.7425.1417.56
ZBM2%12325938943569734.9329.8621.95
ZBL2%13424735941553327.7624.1513.42

Note: , , , , and are the temperature at which 1%, 10%, 30%, 50%, and 70% weight loss occurs, respectively. W600°C, W700°C, and W800°C are the residue of materials at 600, 700, and 800°C.