Type of materialAdsorption capacity for ssDNAReference

Polystyrene beads67 mg/g[26]
Poly(glycidyl methacrylate) beads90 μg/g[27]
Fe3O4 NPs with polyethylene imine69.2 mg/g[28]
Polyethylene glycol dimethacrylate-glycidyl methacrylate65.1 μg/g[29]
Polyethersulfone membranes10 mg/mL[30]
Poly(hydroxyethyl methacrylate)-Fe3O4 MNPs154 mg/g[12]
Immobilized on MNPs as a SPE adsorbent27.86 mg/g[18]
N-Isopropylacrylamide-MNPs83.40 mg/g[13]
Diethylaminoethyl-Magarose as binding8200 ng[31]
Polyglycidyl methacrylate-ethylene glycol dimethacrylate beads1.36 mg/mL[32]