Research Article
In Vivo Study of the Antibacterial Chitosan/Polyvinyl Alcohol Loaded with Silver Nanoparticle Hydrogel for Wound Healing Applications
Figure 6
The rate of wound size reduction measured after 4 days, 8 days, and 12 days (). The asterisk on the bar graph indicates significant difference ().