Research Article

Recyclable Xanthan/TiO2 Composite Cryogels towards the Photodegradation of Cr(VI) Ions and Methylene Blue Dye

Table 1

Compression modulus () and density () values determined for bare XG and XG/TiO2 10% cryogels prepared at pH 2.0, 4.0, and 7.0. The data represent mean values and standard deviations of triplicate.

(kPa) (kg m-3)
pHXGXG/TiO2 10%XGXG/TiO2 10%

2.0
4.0
7.0