Effect of thermal treatment at 500°C on mechanical property of MDPES-2 composites.
| Heat treatment time (min) | Flexural strength (MPa) | Flexural strength retention ratio (%) | Quality retention ratio (%) |
| 7 | 270 | 84 | 99.7 | 15 | 263 | 82 | 99.4 | 30 | 257 | 80 | 98.9 |
|
|