Research Article
Improving the Mechanical Properties of Red Clay Using Xanthan Gum Biopolymer
Table 6
Correlation analyses of the influencing factors with shear strength parameters.
| Variate | Parameter | | | Significance | Fitting equation | |
| 3 d curing | | 60.791 | 0.004 | | | 0.937 | | 9.992 | 0.091 | | | 0.818 |
| 7 d curing | | 31.899 | 0.001 | | | 0.970 | | 42.219 | 0.023 | | | 0.954 |
| 14 d curing | | 36.049 | 0.009 | | | 0.898 | | 13.220 | 0.070 | | | 0.859 |
| 28 d curing | | 51.608 | 0.006 | | | 0.927 | | 11.295 | 0.081 | | | 0.837 |
| 0.0% XG | | 22.206 | 0.042 | | | 0.876 | | 5.437 | 0.290 | | | 0.747 |
| 0.5% XG | | 10.753 | 0.082 | | | 0.765 | | 7.404 | 0.252 | | | 0.810 |
| 1.0% XG | | 22.010 | 0.043 | | | 0.875 | | 2.521 | 0.407 | | | 0.504 |
| 1.5% XG | | 20.032 | 0.046 | | | 0.864 | | 45.376 | 0.104 | | | 0.967 |
| 2.0% XG | | 244.49 | 0.004 | | | 0.988 | | 53.399 | 0.096 | | | 0.972 |
|
|
Note: means very significant; means significant; means not significant. |