SEM images of pristine 25/75 PCL/PHBV scaffold and 25/75 PCL/PHBV with surface modification and with local pores before and after 30 days of degradation under different conditions.

SampleDay 0Day 30
37°C50°CWith enzyme, 37°C

25/75 PCL/PHBV

1H25/75 PCL/PHBV

50NaCl_1H25/75 PCL/PHBV