Research Article
Effect of the Addition of Oil Palm Mesocarp Fibers on the Physical and Mechanical Properties of a Polyester Matrix Composite
Table 3
Densities and porosity rate of the different samples.
| Densities and porosity rate | UP-100 | UP-OPMF-2.5 | UP-OPMF-5 | UP-OPMF-7.5 | UP-OPMF-10 | UP-OPMF-12.5 | UP-OPMF-15 |
| (kg/m3) | 1192.5 | 1182.7 | 1176.6 | 1170.9 | 1165.4 | 1157.8 | 1153.1 | SD | 7.2 | 10.9 | 14.7 | 18.3 | 19.4 | 27.9 | 14.8 | (kg/m3) | 1219.6 | 1216.2 | 1214.2 | 1209.6 | 1203.1 | 1198.4 | 1194.4 | SD | 8.9 | 9.3 | 12.4 | 8.7 | 13.3 | 6.4 | 5.0 | (kg/m3) | 1219.6 | 1219.2 | 1218.9 | 1218.6 | 1218.2 | 1217.9 | 1217.5 | Porosity rate | 2.216 | 2.750 | 3.099 | 3.131 | 3.197 | 3.388 | 3.462 | SD | 0.81 | 0.85 | 0.84 | 0.48 | 0.69 | 0.23 | 0.34 |
|
|
: apparent density; : true density; : theoretical density. |