Range analysis of thickness reduction and thinness reduction data.

FactorsMaximum thinning rate/%Maximum thickening rate/%

88.6499.7495.8189.4718.9516.3516.7818.12
94.5494.1794.8990.7717.0818.0517.1517.40
97.8787.1490.35100.8115.3616.7217.4615.87
29.5533.2531.9429.826.325.455.596.04
31.5131.3931.6330.265.696.115.725.80
32.6229.0530.1233.605.125.575.825.29
3.084.201.823.781.200.660.230.75

Optimal levels

Primary and secondary order

Optimal combination