Facile Controlling of the Physical Properties of Zinc Oxide and Its Application to Enhanced Photocatalysis
Table 2
Textural properties of as-prepared ZnO samples.
| Sample | Eg (eV) | Average crystallite size D (nm) | SBET (m2/g) | BJH pore volume (cm3/g) | Average pore width (nm) |
| CF-ZnO | 3.226 | 17.3 | 16.1 | 0.155 | 26.9 | RF-ZnO | 3.127 | 17.5 | 24.4 | 0.408 | 47.9 | R-ZnO | 3.190 | 22.5 | 18.1 | 0.314 | 53.1 | N-ZnO | 3.207 | 17.8 | 26.4 | 0.481 | 53.7 |
|
|