Research Article
Multiphysical Models for Hydrogen Production Using NaOH and Stainless Steel Electrodes in Alkaline Electrolysis Cell
Table 7
Parameters specific to the experiment on the types of electrolyte at 40 wt%.
| Symbol | Description | Value | Unit |
| | of NaOH + tap water at 80°C | 90.83 | S/m | | of NaOH + AC water at 80°C | 90.83 | S/m | | of NaOH + pressing water at 90°C | 108.33 | S/m | | of NaOH + factory water at 90°C | 108.33 | S/m | | Distance between the anode and the membrane | 0.005 | m | | Distance between the cathode and the membrane | 0.005 | m | | Void fraction of NaOH + tap water at 80°C | 0.2 | — | | Void fraction of NaOH + AC water at 80°C | 0.12 | — | | Void fraction of NaOH + pressing water at 90°C | 0.35 | — | | Void fraction of NaOH + factory water at 90°C | 0.29 | — | C1 | Voltage drop for NaOH + tap water at 80°C | −1.7087 | V | C2 | Voltage drop for NaOH + AC water at 80°C | −1.5259 | V | C3 | Voltage drop for NaOH + pressing water at 90°C | −2.0872 | V | C4 | Voltage drop for NaOH + factory water at 90°C | −1.8505 | V | k1 | Correction factor for NaOH + tap water at 80°C | 0.034 | — | k2 | Correction factor for NaOH + AC water at 80°C | 0.032 | — | k3 | Correction factor for NaOH + pressing water at 90°C | 0.033 | — | k4 | Correction factor for NaOH + factory water at 90°C | 0.033 | — |
|
|