Photodegradation of Methyl Green by Nickel-Dimethylglyoxime/ZSM-5 Zeolite as a Heterogeneous Catalyst
Figure 9
Effect of the initial dye concentration on decolorization efficiency of MG; 0.6 g L−1 of catalyst; initial solution pH, 5.3; 55 W Hg lamp; continuous stirring; irradiation time, 180 min; room temperature.