Research Article
Application of Functionalized SWCNTs for Increase of Degradation Resistance of Acrylic Paint for Cars
Table 3
Thickness of the final layer.
| Sample | (m) | Sample | (m) | Sample | (m) |
| P1SWOH1 | 108.41 | P1SWFC1 | 104.48 | P1SW1 | 111.20 | P1SWOH2 | 83.44 | P1SWFC2 | 108.08 | P1SW2 | 136.63 | P1SWOH3 | 91.52 | P1SWFC3 | 122.94 | P1SW3 | 139.25 | P1SWOH4 | 76.28 | P1SWFC4 | 109.12 | P1SW4 | 160.88 | P1SWOH5 | 73.45 | P1SWFC5 | 118.11 | P1SW5 | 157.48 |
|
|