Research Article

Size Control of Iron Oxide Nanoparticles Using Reverse Microemulsion Method: Morphology, Reduction, and Catalytic Activity in CO Hydrogenation

Figure 3

Adsorption BJH pore size distribution of prepared catalysts after calcinations ((a) HLB = 13.9, (b) HLB = 23.7, (c) HLB = 31.2, and (d) HLB = 40).
781595.fig.003a
(a)
781595.fig.003b
(b)
781595.fig.003c
(c)
781595.fig.003d
(d)