Reduction of Magnetite in the Presence of Activated Carbon Using Mechanical Alloying
Figure 2
Room temperature MAS spectra of the ball-milled magnetite and graphite mixtures (1 : 3 mole ratio) at different ball to powder ratios (BPR), while rotational speed and milling periods were kept constant at 400 rpm and 20 hours, respectively.