Research Article

Catalytic Performance of Fe-Mn/Si Nanocatalysts for CO Hydrogenation

Table 3

N2 adsorption-desorption measurements of iron-manganese catalyst treated with H2S.

H2S volume fractionsaSpecific surface area (m2 g−1)Pore diameter ( )Pore volume (cm3 g−1)

205.746.40.31
2/100225.647.90.37
4/100228.549.30.39
6/100233.553.20.42
8/100228.351.50.39
10/100219.750.40.38
12/100213.947.90.34

aH2S volume fractions = .