Research Article

Synthesis and Characterization of Ag2S Layers Formed on Polypropylene

Figure 5

X-ray diffractograms of the Ag2S layers formed on PP in 0.08 mol/dm3 AgNO3 and 0.20 mol/dm3 Na2S2O3 solutions at 20°C for different immersions time, min: 1: 40; 2: 140; 3: 200.
987879.fig.005