Research Article

Anodic Dissolution of API X70 Pipeline Steel in Arabian Gulf Seawater after Different Exposure Intervals

Figure 2

EIS Nyquist plots obtained for the API X70 pipeline steel after its immersion for (a) 1 h and (b) 20 h in Arabian Gulf seawater.
753041.fig.002