Research Article

Structural and Electrochemical Properties of Lithium Nickel Oxide Thin Films

Figure 2

XRD patterns of (a) as-deposited, (b) 400°C, (c) 500°C, and (d) 600°C annealed LiNiO2 thin films. The annealing time was 10 minutes.
824083.fig.002