Research Article
Reduction of Polymer Waste Pyrolysis Fractions over Pt/Al2O3 with Methanol Decomposition Hydrogen to Obtain Fuel-Grade Hydrocarbons
Table 2
Results of the reduction of fraction F1 over 5% Pt/
-Al
2O
3 with gaseous hydrogen and hydrogen from methanol decomposition.
(a) |
| Fraction composition | | Before hydrogenation reactions | | Contents [%] | Total [%] |
| Saturated hydrocarbons | C8–C19 | 31.2 | 43.4 | C20–C25 | 12.2 |
| Unsaturated hydrocarbons | C8–C19 | 56.6 | 56.6 | C20–C25 | 0.0 |
|
|
(b) |
| Temp. |
Hydrogenation with hydrogen |
Hydrogenation with hydrogen from methanol decomposition | Contents [%] | Total [%] | Contents [%] | Total [%] |
| 100 | 35.2 | 60.6 | 38.7 | 58.3 | 25.4 | 19.6 | 39.4 | 39.4 | 34.5 | 41.7 | 0.0 | 7.2 |
| 200 | 53.4 | 74.1 | 48.6 | 78.4 | 20.7 | 29.8 | 25.9 | 25.9 | 18.1 | 21.6 | 0.0 | 3.5 |
| 300 | 78.8 | 94.1 | 59.7 | 95.7 | 15.3 | 36.0 | 5.9 | 5.9 | 4.3 | 4.3 | 0.0 | 0.0 |
| 400 | 37.2 | 80.5 | 56.4 | 91.2 | 43.3 | 34.8 | 12.8 | 12.8 | 5.1 | 5.1 | 0.0 | 0.0 |
|
|