Research Article
Anticorrosion Nanocrystalline Beta Zeolite Thin Film for Advanced Applications
Table 2
Corrosion parameters derived from the polarization curves of bare and coated alloy plates in NaCl, H2SO4, and NaOH solutions.
| Sample ID | (V/SCE) | (A/cm2) | Corrosion rate (mm/year) |
| 3 wt% NaCl solution | | | | TC1010 | −543.51 | −3.52 | 0.0034593 | BZTC1010 | −660.2 | −3.54 | 0.0032988 | 0.1 M H2SO4 solution | | | | TC1010 | −517.61 | −0.82 | 1.7257 | BZTC1010 | −498.62 | −1.41 | 0.4526569 | 0.1 M NaOH solution | | | | TC1010 | −297.33 | −3.28 | 0.0059535 | BZTC1010 | −244.39 | −3.83 | 0.0016986 |
|
|