Research Article
Effect of Graphene Nanosheets on the Morphology, Crystallinity, and Thermal and Electrical Properties of Super Tough Polyamide 6 Using SEBS Compounds
Table 3
Mechanical properties of samples.
| Sample | Impact strength (kJ/m2) | Elongation at break (%) | Tensile strength (MPa) | Modulus (MPa) |
| PA6 | 4.26 ± 0.4 | 60.3 ± 1.6 | 64.3 ± 3 | 1208.6 ± 21.7 | M0 | 4.9 ± 0.2 | 70.7 ± 3 | 44.9 ± 0.8 | 939.3 ± 4.4 | M2 | 11.13 ± 0.6 | 145.3 ± 8.4 | 36.1 ± 3 | 858.5 ± 17.4 | M4 | 13.71 ± 0.6 | 179.6 ± 3 | 36.2 ± 0.6 | 830 ± 14.5 | M6 | 14.96 ± 0.5 | 224 ± 1.6 | 37.9 ± 0.3 | 901 ± 4.1 | M10 | 13.5 ± 0.9 | 148.3 ± 9.9 | 38.7 ± 2.9 | 797 ± 14 |
|
|