Research Article
Stress Corrosion Cracking of a Forged Mg-Al-Zn Alloy with Different Surface Conditions
Figure 8
SEM micrographs of the AQ80M alloy with MAO coating under different strains: (a) 0.3σ0.2 × 120 h, (b) 0.45σ0.2 × 120 h, (c) 0.6σ0.2 × 120 h, (d) 0.75σ0.2 × 120 h, (e) 0.75σ0.2 × 120 h, and (f) 0.75σ0.2 × 240 h.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |