Research Article
Effect of Recycled Rubber on the Properties of Road Bitumen
Table 1
Bitumen modification at 190°C.
| Sample no. | Modifiers (%) | Modification time (h) | Residue after devulcanization (%) | Rubber 0.4 | Rubber 0.8 | PB solution | Sulfur donor |
| 1 | 10 | — | 3 | 0.07 | 2 | 7.2 | 2 | 10 | — | 3 | 0.07 | 4 | 5.9 | 3 | — | 10 | 3 | 0.07 | 8 | 6.1 | 4 | 10 | — | 3 | 0.07 | 16 | 4.5 | 5 | — | — | 3 | 0.07 | 2 | 1.8 | 6 | — | — | 10 | 0.07 | 2 | 2.6 |
|
|