Research Article
Effect of Recycled Rubber on the Properties of Road Bitumen
Table 2
Bitumen modification at 220°C.
| Sample no. | Modifiers (%) | Modification time (h) | Residue after devulcanization (%) | Rubber 0.4 | Rubber 0.8 | PB solution | Sulfur donor |
| 7 | 15 | — | 3 | 0.07 | 2 | 5.3 | 8 | 15 | — | 3 | 0.07 | 4 | 4.0 | 9 | — | 15 | 3 | 0.07 | 4 | 5.3 | 10 | 15 | — | 3 | 0.07 | 8 | 3.4 | 11 | — | 15 | 3 | 0.07 | 8 | 3.8 | 12 | 15 | — | 3 | 0.07 | 16 | 2.8 | 13 | — | 15 | 3 | 0.07 | 16 | 3.7 |
|
|