TGA and DSC results of the P(DEAMSt) and P(DEAMSt-co-MMA).

Polymer systems (°C)
Initial decomposition temp. (°C)Final decomposition temp. (°C)50% weight loss temp (°C)(%) residue at 500 (°C)

P(DEAMSt0.11-co-MMA)1132134093388
P(DEAMSt0.19-co-MMA)10521941032914
P(DEAMSt0.30-co-MMA)932284003397
P(DEAMSt)8022941034019