Specific surface areas of STi samples.

CatalystsBET (m2/g)Pore volume (cm3/g)Average pore width (nm)

SrTiO330.020.1114.76
Ti30.080.1216.59
Ti30.770.1317.47
Ti31.090.1520.89
Ti28.160.0919.87
Ti25.240.0819.31