Research Article

Nanoscale Morphological Changes at Lithium Interface, Triggered by the Electrolyte Composition and Electrochemical Cycling

Figure 2

Bode phase (a) and total impedance (b) diagrams for anodes tested in symmetric cell, after 20 h contact time with the electrolyte 1 M LiTFSI, DOL/TEGDME (7 : 3) (black); 1 M LiTFSI, 0.2 M LiNO3, DOL/TEGDME (7 : 3) (red); 1 M LiTFSI, PS DOL/TEGDME (7 : 3) (green); and 1 M LiTFSI, 0.2 M LiNO3, PS DOL/TEGDME (7 : 3) (blue).
(a)
(b)