Electrochemical Removal of Humic Acids from Water Using Aluminum Anode: Influence of Chloride Ion and Current Parameters
Table 2
Experimental parameters and corresponding energy consumption for 90% HA removal: starting concentration = 50 mg·L−1, volume = 0.5 L.
| Number of the experiment | Electrolyte | Current density (A·m−2) | Current intensity (A) | Voltage (V) | Time (min) | Energy (joule) |
| 1 | NaCl 0.001 M | 10 | 0.075 | 6.1 | 30 | 824 | 2 | NaCl 0.08 M | 10 | 0.075 | 1.2 | 15 | 81 | 3 | NaCl 1.5 M | 10 | 0.075 | 0.8 | 10 | 36 | 4 | NaCl 0.001 M | 50 | 0.375 | 25.1 | 15 | 8470 | 5 | NaCl 0.04 M | 50 | 0.375 | 2.8 | 50 | 3150 | 6 | NaCl 0.08 M | 50 | 0.375 | 2.2 | 20 | 990 | 7 | NaCl 1.5 M | 50 | 0.375 | 1.0 | 10 | 225 | 8 | NaCl 0.001 M | 100 | 0.75 | 3.0 | 15 | 1890 | 9 | NaCl 0.08 M | 100 | 0.75 | 2.2 | 10 | 924 | 10 | NaCl 1.5 M | 100 | 0.75 | 1.1 | 10 | 462 | 11 | NaNO3 0.08 M | 10 | 0.075 | 3.5 | 90 | 1418 | 12 | NaNO3 0.08 M | 50 | 0.375 | 4.3 | 100 | 9675 | 13 | NaNO3 0.08 M | 100 | 0.75 | 5.3 | 10 | 2226 |
|
|