Research Article
Reaction Kinetics of Chlorine Corrosion to Heating Surfaces during Coal and Biomass Cofiring
Table 4
The conversion rate of metal specimens at different times.
| t(°C) | α | 0 | 6 h | 12 h | 16 h | 24 h | 30 h |
| 500 | 0 | 0.472 | 0.735 | 0.849 | 0.906 | 1.000 | 550 | 0 | 0.438 | 0.650 | 0.775 | 0.913 | 1.000 | 600 | 0 | 0.454 | 0.672 | 0.798 | 0.932 | 1.000 | 650 | 0 | 0.442 | 0.693 | 0.847 | 0.939 | 1.000 |
|
|