Photocatalytic degradation efficiency of MO in different samples under sunlight and sunlight (H2O2) conditions.
| Sunlight (H2O2) and sunlight (min) | TiO2 (%) | 1 wt % (%) | 3 wt % (%) | 5 wt % (%) | 7 wt % (%) | 9 wt % (%) |
| 30 | 12.64 5.32 | 22.29 6.80 | 28.53 7.71 | 39.03 10.36 | 35.32 9.13 | 31.89 8.29 | 60 | 28.97 10.79 | 37.98 14.65 | 45.31 15.29 | 56.94 21.24 | 51.97 18.59 | 49.32 17.09 | 90 | 42.37 17.03 | 50.01 22.87 | 64.32 24.29 | 77.07 33.09 | 72.09 30.26 | 68.29 28.67 | 120 | 59.24 26.29 | 70.26 33.27 | 77.91 35.76 | 98.90 46.97 | 89.46 42.97 | 81.08 39.08 |
|
|