Evaluation of Oxidation Performance of TRISO Fuel Particles for Postulated Air-Ingress Accident of HTGR
Figure 4
XRD patterns of TRISO particles. (a) Both as-deposited sample and the samples after air oxidation for 24 h at 1200°C–1400°C and (b) amplified XRD patterns from 18°–30°.