Research Article

Comparison of 304 SS, 2205 SS, and 410 SS Corrosion by Sulfate-Reducing Desulfovibrio ferrophilus

Figure 1

Three-electrode electrochemical glass cells at day 0 (a) and at the end of 7-day incubation (b). Note: the left wire was for the counterelectrode and the right wire for the working electrode. The center glass tube was for the reference electrode.
(a)
(b)