Research Article
Comparison of 304 SS, 2205 SS, and 410 SS Corrosion by Sulfate-Reducing Desulfovibrio ferrophilus
Figure 2
Surface images of 3 stainless steel types after 7-day incubation: (a) 304 SS, (b) 410 SS, and (c) 2205 SS. Note: red bar indicates IFM scan path in Figure 3(b).