Review Article

Combustion Characteristics of Nanoaluminium-Based Composite Solid Propellants: An Overview

Figure 6

SEM/TEM micrographic images of nanoaluminized samples quench collected at 4 MPa from the propellants of various coarse and fine AP sizes: (a) 250 and 75 μm; (b) 350 and 75 μm; (c) 450 and 53 μm; (d) 450 and 75 μm.