Research Article
Synthesis and Characterization of Magnetic Fe3O4/Zeolite NaA Nanocomposite for the Adsorption Removal of Methylene Blue Potential in Wastewater Treatment
Figure 7
UV-VIS absorbance spectra of supernatants collected from batch adsorption experiments. (a) The absorbance spectra of the MB solution treated by Fe3O4/ZA nanocomposite with different Fe3O4 NP loadings; (b, c) absorbance spectra of 3.3% Fe3O4/ZA and 6.6% Fe3O4/ZA samples at different interaction (adsorption) times; (d) removal efficiency (R, %) and adsorption capacity (, mg·g−1) of 3.3% Fe3O4/ZA and 6.6% Fe3O4/ZA samples, respectively; linear fitting results of removal efficiency and adsorption capacity in adsorption ranges of 0–60 minutes (e) and 60–240 minutes (f) in (d); the experiments data are presented as solid dots with error bars, while solid lines are linear fitting results of experiments data in Figures 7d, 7e, and 7f.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |