Facile One-Step Flame Synthesis of La1−xSrxMnO3 Nanoparticles for CO Catalytic Oxidation
Table 7
Temperature values of 50% and 90% conversion in CO catalytic oxidation of mixture atmosphere.
| Case2 catalytic cycles | LaMnO3 | La0.8Sr0.2MnO3 | La0.6Sr0.4MnO3 | La0.4Sr0.6MnO3 | La0.2Sr0.8MnO3 | T50 | T90 | T50 | T90 | T50 | T90 | T50 | T90 | T50 | T90 |
| 1st | 181.8 | 209.2 | 167.1 | 197.2 | 167.7 | 196.6 | 153.1 | 181.5 | 154.3 | 188.7 | 2nd | 175.9 | 212.1 | 172.8 | 203 | 164.7 | 196.7 | 152.8 | 182.9 | 158.3 | 192.4 | 3rd | 181.3 | 220.3 | 171.5 | 203.8 | 174.2 | 206.9 | 154.6 | 188.4 | 157.1 | 193.8 | 4th | 174.2 | 214.8 | 168.9 | 201.4 | 169.9 | 203.9 | 154.9 | 185.6 | 156.1 | 194.3 | 5th | 185.2 | 223.8 | 170.5 | 201.6 | 173.5 | 206.6 | 164.2 | 194.6 | 162.3 | 199.6 |
|
|