Research Article

Assessment of Some Characteristics and Properties of Zirconium Dioxide Nanoparticles Modified with 3-(Trimethoxysilyl) Propyl Methacrylate Silane Coupling Agent

Table 1

Composition and designation of modified ZrO2 nanoparticles.

No.CompositionDesignationWeight
(g)msilan (mg)

1ZrO2u-ZrO250
2ZrO2 + 3 wt.% MSPMSm-ZrO2-3515
3ZrO2 + 5 wt.% MSPMSm-ZrO2-5525
4ZrO2 + 7 wt.% MSPMSm-ZrO2–7535
5ZrO2 + 10 wt.% MSPMSm-ZrO2–10550
6ZrO2 + 15 wt.% MSPMSm-ZrO2–15575