Research Article
Upgradation of Iron Ore Fines and Slime by Selective Flocculation Using Surface-Active Agents, Settling Study, and Characterization of the Beneficiation Waste for Value Addition
Figure 9
Al2O3/Fe and Al2O3/SiO2 ratios in the concentrate from 25 wt. % slurry of slime at different doses of AD 200 at pH 8.