Particle size distribution of feed.

Size analysis

Sample−10 + 8 mm−8 + 6.5 mm−6.5 + 4 mm−4 + 2 mm−2 + 1 mm−1 + 0.5 mm−0.5 + 0.25 mm−0.25 mm
Iron ore fines9.486.7410.3622.7710.4418.628.6712.92
Tailings+70 μm−70 + 50 μm−50 + 40 mm−40 + 20 μm−20 + 10 μm−10 μm
4.902.281.7511.3727.4852.22