Research Article

Upgradation of Iron Ore Fines and Slime by Selective Flocculation Using Surface-Active Agents, Settling Study, and Characterization of the Beneficiation Waste for Value Addition

Table 4

Values of the parameters of equation (1) for beneficiation of 10 wt. % slurry of fines.

ExperimentSystemRate constant (k) in min−1Half-life time (t1/2) in min.YoPlateauGoodness of fit (R2)

Stability of suspension in 10 wt. % slurry of fines (Figure 3)AD 200 ppm 5, pH 80.067910.202.6970.91800.9462
AD 200 ppm 10, pH 80.07369.4103.3721.0510.9861
AD 200 ppm 15, pH 80.08138.5183.7991.1790.9861
Sodium humate (0.05 wt. %), pH 80.046314.954.2321.4860.9824
Without additive, pH 80.34691.9984.7280.68460.9786