Research Article

Upgradation of Iron Ore Fines and Slime by Selective Flocculation Using Surface-Active Agents, Settling Study, and Characterization of the Beneficiation Waste for Value Addition

Table 5

Values of the parameters of equation (1) for beneficiation of 10 wt. % slurry of fines.

ExperimentSystemRate constant (k) in min−1Half-life time (t1/2) in min.YoPlateauGoodness of fit (R2)

Stability of suspension in 10 wt. % slurry of iron ore fines (Figure 5)With 0.05% humate, pH 80.046314.954.2321.4860.9824
With (0.05% humate + 5% starch), pH 80.068810.074.2031.6860.9656
With (0.05% humate + 10% starch), pH 80.064210.794.0151.5290.9675
With (0.01% humate + 5% starch), pH 80.061611.253.5171.0630.9800
With (0.01% humate + 10% starch), pH 80.066310.453.7471.1430.9881
Without additive, pH 80.34691.9984.7280.68460.9786