Values of the parameters of equation (1) for beneficiation of 10 wt. % slurry of slime.

ExperimentSystemRate constant (k) in min−1Half-life time (t1/2) in min.YoPlateauGoodness of fit (R2)

Stability of suspension in 10 wt. % slurry of slime (Figure 6)With 0.05% humate, pH 80.050313.766.6720.99350.9979
With (0.05% humate + 5% starch), pH 80.046214.986.9291.2450.9961
With (0.05% humate + 10% starch), pH 80.045315.297.0171.1880.9981
With (0.01% humate + 5% starch), pH 80.053412.976.1600.94560.9953
With (0.01% humate + 10% starch), pH 80.047814.506.3581.0150.9973
Without additive, pH 80.050113.845.5350.84330.9956