Research Article

Optimization of Laser Transmission Joining Process Parameters on Joint Strength of PET and 316 L Stainless Steel Joint Using Response Surface Methodology

Figure 3

Microstructure of joint seam width of 316 L stainless steel and PET joint.
197060.fig.003a
(a)
197060.fig.003b
(b)
197060.fig.003c
(c)
197060.fig.003d
(d)
197060.fig.003e
(e)
197060.fig.003f
(f)